SCHOTT ARTISTA® extra-clear decorative glass  is made from the finest quality low-iron sheet glass. The crystal-like clarity of the glass showcases the interior and makes the space appear larger. The subtle structured pattern brings life and sparkle to the room.

SCHOTT ARTISTA® brilliant is the new extra-clear glass from SCHOTT. It offers features similar to those of ARTISTA® but with a less structured surface. Outstanding brilliance and 100% fusing compatibility are the main characteristics of ARTISTA® brilliant.
Summary:
  • ARTISTA® is made from finest quality low-iron sheet glass
  • ARTISTA® and ARTISTA® brilliant are crystal clear
  • ARTISTA®  brilliant  is less structured
  • offers various applications for both interior and exterior
  • compatible for fusing applications
  • wide range of glass manufacturing options

Benefits

SCHOTT ARTISTA® - extra-clear decorative glass is unique due to ...
  • glass with extra-clear properties
  • structured on one side
  • 2 different surface variations available: ARTISTA® clear and ARTISTA®  brilliant 
  • available for fusing applications
  • suited for stained glass applications
  • wide range of glass manufacturing options (e.g. as laminated glass or insulating glass)
SCHOTT ARTISTA® clear glass: its subtle structured pattern brings life and sparkle to the room.
Timeless structure of SCHOTT ARTISTA®

Area of Applications

Architecture Interior
  • furniture
  • separation walls
  • shower doors
Art and Design
  • fusing
  • art installations
  • chandeliers

Technical Information

Variety of glazing options

SCHOTT ARTISTA® extra-clear decorative glass can be processed the same way as conventional glass - either as laminated glass or insulation glass. This opens up a variety of additional functions ranging from thermal to sound insulation.

ARTISTA® extra-clear decorative glass offers diverse application possibilities for both interior and exterior use:
  • as a full pane
  • in stained glass or
  • as a fused glass
Nominal thickness Tolerance Dimensions
  2.75 mm ± 0.25 mm 1,000 x 1,500 mm
1,600 x 1,500 mm
2,100 x 1,500 mm
  4.0 mm ± 0.25 mm 1,800 x 1,500 mm
2,100 x 1,500 mm
  6.0 mm ± 0.50 mm 1,000 x 1,500 mm
2,100 x 1,500 mm
2,400 x 1,500 mm
  8.0 mm ± 0.50 mm 2,100 x 1,500 mm
10.0 mm ± 0.50 mm 2,100 x 1,500 mm
2,400 x 1,500 mm

Contact

If you have a product inquiry, questions for service & support or other topics for SCHOTT ARTISTA®, please click the contact button. You will be forwarded to our contact form.
If you are looking for an Architectural Partner in your region, please click on the Architectural Partner Logo. You will be forwarded to our Partner Contact page.
Click here and find an Architectural Partner in your region.
Modifier
Sur ce site Web, SCHOTT utilise des cookies afin d'optimiser l'affichage des pages et améliorer le confort et l'expérience de l'utilisateur. En continuant à naviguer sur ce site, vous déclarez les accepter.