PYRANOVA®Superior quality and clarity

Summary

PYRANOVA® for exterior applications – At a glance

Key facts

PYRANOVA® for exterior applications

PYRANOVA® for exterior applications is a special glass for use in external or particulary difficult situations, a clear composite safety glass for fire resistant glazing that offers fire resistant properties in accordance with DIN EN ISO 12543.
Depending on its structure, it is manufactured from at least two float glass panes with transparent, fire resistant intumescent interlayers and an external pane made of laminated safety glass.

Technical data

Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
  acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Exterior
PYRANOVA® EW EI 15 / EW 30
10
24
87
5.4
36
PYRANOVA® EW EI 15 / EW 30
14
32
86
5.2
38
PYRANOVA® 30 EI 30
19
44
83
5
38
PYRANOVA® 45 EI 45 / EW 60
19
44
85
5
38
PYRANOVA® 60 EI 60
27
61
86
4.7
41
PYRANOVA® 90 EI 90
40
93
83
4.1
44
PYRANOVA® 120 EI 120
54
116
74
2.5
44

Contact

Mr. Martin Brown

SCHOTT UK Ltd.

Drummond Road
ST16 3EL Stafford
United Kingdom

 +44 (0)1785/223166
 +44 (0)1785/223522

At a glance

Areas of application

PYRANOVA® Spezialglas eignet sich für alle Anwendungsbereiche, in denen im Brandfall eine thermische Isolation notwendig ist.

SCHOTT ist mit über 30 Jahren umfangreicher Erfahrung im Brandschutzmarkt kompetent und innovativ zugleich. Gemeinsam mit Systempartnern entwickelt die SCHOTT Technical Glass Solutions GmbH Konstruktionen mit PYRANOVA® Spezialglas, die international zugelassen und hervorragend geeignet sind für den Einsatz in Türen, Fassaden und Trennwänden, unter anderem in Fluchtwegen und Treppenhäusern.

Product types

PYRANOVA® for exterior applications

PYRANOVA® for exterior applications is a special glass for use in external or particulary difficult situations, a clear composite safety glass for fire resistant glazing that offers fire resistant properties in accordance with DIN EN ISO 12543.
Depending on its structure, it is manufactured from at least two float glass panes with transparent, fire resistant intumescent interlayers and an external pane made of laminated safety glass.

PYRANOVA® for exterior applications – Technical data

TECHNICAL INFORMATION
Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
  acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Exterior
PYRANOVA® EW EI 15 / EW 30
10
24
87
5.4
36
PYRANOVA® EW EI 15 / EW 30
14
32
86
5.2
38
PYRANOVA® 30 EI 30
19
44
83
5
38
PYRANOVA® 45 EI 45 / EW 60
19
44
85
5
38
PYRANOVA® 60 EI 60
27
61
86
4.7
41
PYRANOVA® 90 EI 90
40
93
83
4.1
44
PYRANOVA® 120 EI 120
54
116
74
2.5
44

Mr. Martin Brown

SCHOTT UK Ltd.

Drummond Road
ST16 3EL Stafford
United Kingdom

 +44 (0)1785/223166
 +44 (0)1785/223522