SCHOTT PYRAN®Superior quality and clarity

Summary

At a glance

Superior safety glass

PYRAN® fire resistant glazing made of borosilicate is far superior to conventional safety glasses with a soda-lime composition:

  • High ability to withstand temperature differentials: Compared to other products, tempered borosilicate glass withstands temperature differentials much better and can thus be glazed with normal edge cover (15 ± 2 mm).
  • Higher softening temperature: Due to the fact that the glass is self-supporting for over 30 minutes, large panes and relatively basic frame constructions are now possible.
  • Higher viscosity: Due to the low flow behavior that results from the high viscosity of borosilicate glass, longer fire resistance times in excess of 90 minutes can be achieved with more edge cover.
  • No forming of NiS crystals: The chemical composition of borosilicate glass is such that NiS crystals are unable to form. This means a sudden fracture caused by embedded NiS crystals can be ruled out with PYRAN®.

Proven and safe

PYRAN® remains transparent, even under high thermal loads. This ensures vital insight in the case of a fire and makes it much easier to evacuate a burning building safely. Excellent color reproduction and high transmission in the visible and UV range ensure that this increase in security is not achieved at the expense of appearance. It is certainly no coincidence that PYRAN® has been proving itself in airports, hospitals, hotels, industrial buildings, museums, offices, schools, shopping centers, sports facilities and even on cruise ships for decades.

Key facts

  • Permanent transparency
  • Integrity up to 120 minutes
  • Thickness range from 6 to 12 mm
  • Max. Dimensions 1800 mm x 3600 mm (thickness >/= 8mm)
  • Safety glass
  • Multifunctional
  • Borosilicate glass as basis material

Technical data

Product Fire Rating Thickness Weight Ug-Value g-Value Light Trans- mission Sound Reduction
  acc. EN 13501 [mm] [kg/m2] [k/Wm2] [%] [%] [dB]
PYRAN® S E(G) 30 - 120 6 13.7 5.8 91 92 31
E(G) 30 - 120 8 18.2 5.8 90 92 32
E(G) 30 - 120 10 22.8 5.8 90 92 33
E(G) 30 - 120 12 27.4 5.8 90 92 34
Double glazing units
ISO PYRAN® S E(G) 30 24   2.7 78 83 33
E(G) 30 26   2.7 75 82 34
E(G) 30 - 90 25   2.7 78 83 33
E(G) 30 - 90 27   2.7 75 82 34
Heat insulation - Low e coatings
ISO PYRAN® S E(G) 30 24   1.4 61 82 33
E(G) 30 24   1.4 65 82 33
E(G) 30 - 90 25   1.4 61 82 34
E(G) 30 - 90 25   1.4 65 82 34
ISO PYRAN® S-D E(G) 30 - 60 28   1.4 55 79  
E(G) 30 - 60 28   1.4 64 79  
E(G) 30 - 60 30   1.4 54 78 39
E(G) 30 - 60 30   1.4 64 78 39
Sun protection - Solar control coatings
ISO PYRAN® S E(G) 30 26   1.4 27 50 34
E(G) 30 26   1.4 22 41 34
E(G) 30 26   1.4 17 30 34
E(G) 30 26   1.4 30 47 34
E(G) 30 - 90 26   1.4 27 50 33
E(G) 30 - 90 26   1.4 22 41 33
E(G) 30 - 90 26   1.4 17 30 33
E(G) 30 - 90 26   1.4 30 47 33
Sound insulation
ISO PYRAN® S-D E(G) 30 - 60 35   2.7     42
E(G) 30 - 60 30   1.4 54 78 39
E(G) 30 - 60 30   2.7     41
E(G) 30 - 60 45   2.7     43
E(G) 30 - 60 45   2.7     43
E(G) 30 - 60 34   2.7     45

Contact

Mr. Martin Brown

SCHOTT UK Ltd.

Drummond Road
ST16 3EL Stafford
United Kingdom

 +44 (0)1785/223166
 +44 (0)1785/223522

At a glance

Superior safety glass

PYRAN® fire resistant glazing made of borosilicate is far superior to conventional safety glasses with a soda-lime composition:

  • High ability to withstand temperature differentials: Compared to other products, tempered borosilicate glass withstands temperature differentials much better and can thus be glazed with normal edge cover (15 ± 2 mm).
  • Higher softening temperature: Due to the fact that the glass is self-supporting for over 30 minutes, large panes and relatively basic frame constructions are now possible.
  • Higher viscosity: Due to the low flow behavior that results from the high viscosity of borosilicate glass, longer fire resistance times in excess of 90 minutes can be achieved with more edge cover.
  • No forming of NiS crystals: The chemical composition of borosilicate glass is such that NiS crystals are unable to form. This means a sudden fracture caused by embedded NiS crystals can be ruled out with PYRAN®.

Proven and safe

PYRAN® remains transparent, even under high thermal loads. This ensures vital insight in the case of a fire and makes it much easier to evacuate a burning building safely. Excellent color reproduction and high transmission in the visible and UV range ensure that this increase in security is not achieved at the expense of appearance. It is certainly no coincidence that PYRAN® has been proving itself in airports, hospitals, hotels, industrial buildings, museums, offices, schools, shopping centers, sports facilities and even on cruise ships for decades.

Areas of application

Whether fitted in timber or steel structures, SCHOTT Technical Glass Solutions in cooperation with system partners develop doors with PYRAN® which are excellently suited and approved for sale in markets outside of Germany*.

*The German building code does not list G (E) doors.

Product types

  • Permanent transparency
  • Integrity up to 120 minutes
  • Thickness range from 6 to 12 mm
  • Max. Dimensions 1800 mm x 3600 mm (thickness >/= 8mm)
  • Safety glass
  • Multifunctional
  • Borosilicate glass as basis material

Technical data

TECHNICAL INFORMATION
Product Fire Rating Thickness Weight Ug-Value g-Value Light Trans- mission Sound Reduction
  acc. EN 13501 [mm] [kg/m2] [k/Wm2] [%] [%] [dB]
PYRAN® S E(G) 30 - 120 6 13.7 5.8 91 92 31
E(G) 30 - 120 8 18.2 5.8 90 92 32
E(G) 30 - 120 10 22.8 5.8 90 92 33
E(G) 30 - 120 12 27.4 5.8 90 92 34
Double glazing units
ISO PYRAN® S E(G) 30 24   2.7 78 83 33
E(G) 30 26   2.7 75 82 34
E(G) 30 - 90 25   2.7 78 83 33
E(G) 30 - 90 27   2.7 75 82 34
Heat insulation - Low e coatings
ISO PYRAN® S E(G) 30 24   1.4 61 82 33
E(G) 30 24   1.4 65 82 33
E(G) 30 - 90 25   1.4 61 82 34
E(G) 30 - 90 25   1.4 65 82 34
ISO PYRAN® S-D E(G) 30 - 60 28   1.4 55 79  
E(G) 30 - 60 28   1.4 64 79  
E(G) 30 - 60 30   1.4 54 78 39
E(G) 30 - 60 30   1.4 64 78 39
Sun protection - Solar control coatings
ISO PYRAN® S E(G) 30 26   1.4 27 50 34
E(G) 30 26   1.4 22 41 34
E(G) 30 26   1.4 17 30 34
E(G) 30 26   1.4 30 47 34
E(G) 30 - 90 26   1.4 27 50 33
E(G) 30 - 90 26   1.4 22 41 33
E(G) 30 - 90 26   1.4 17 30 33
E(G) 30 - 90 26   1.4 30 47 33
Sound insulation
ISO PYRAN® S-D E(G) 30 - 60 35   2.7     42
E(G) 30 - 60 30   1.4 54 78 39
E(G) 30 - 60 30   2.7     41
E(G) 30 - 60 45   2.7     43
E(G) 30 - 60 45   2.7     43
E(G) 30 - 60 34   2.7     45