BMW Welt, München
BMW Welt, München

SCHOTT PYRAN®

Summary

PYRAN® S – At a glance

Key facts

PYRAN® S

PYRAN® S is a monolithic, thermally tempered borosilicate safety glass in accordance with DIN EN Standard 13024-1. Thanks to its outstanding optical and mechanical properties, it has a long record of proven performance in many different buildings as a component in fire resistant glazing of the fire resistance classes E 30, E 60, E 90 and E 120.

  • Borosilicatglass
  • Classifications:
  • E 30 to E 120
  • EW 30 to E 60
  • Glass thickness: up to 12 mm

Design and variety of PYRAN® S

    PYRAN® S - Anti-reflective glazing

    PYRAN® S for anti-reflective glazing performs several important functions all at the same time. It offers clear visibility due to low residual reflection and up to 2 hours of additional protection in case of fire. Anti-reflective coated PYRAN® S is a monolithic, thermally toughened borosilicate glass that is anti-reflective on both sides due to the fact that it is manufactured using a dip-coating process. The glass is coated with a hard, weather-resistant and multi-layered interference system. As a result, light reflection of 8% with an uncoated glass can be reduced to 1% using coated borosilicate glass.

    PYRAN® S - Butt joint system

    Butt joint PYRAN® S can be used very easily in demanding architectural designs. With the PYRAN® S butt joint system, for instance, a special silicone joint is used to join the panes of glass together without a frame. This helps create light, smooth sheets of glass that are virtually endless, and guarantees a clear view at all times without any disturbing vertical profiles. Simply ideal for applications in which fire protection needs to be combined with maximum visibility and minimal visual disturbances.

    PYRAN® S - Structural glazing

    Systems that use PYRAN® S for structural glazing require no frame constructions whatsoever. This is the result of a perfect symbiosis between glass panes connected to each other by joints that are barely noticeable and point mounts and brackets that secure the glass panes to a strong, yet light, supporting structure. The panes remain permanently fixed in place, free of tension and without slippage under even the most extreme conditions, such as loads created by internal wind pressure or suction.

    PYRAN® S – Composite safety glass

    PYRAN® S composite safety glass as a laminate made of PYRAN® S and soda lime or single-pane safety glass can be used to meet special requirements for noise protection and protection against falls.
    The use according to TRLV and TRAV is stipulated in the general type approval Z-70.3-145. In addition to certification of protection against falling, there are general type approval test certificates according to TRAV with timber or steel frames.

Technical data

Product Fire Rating Thickness Weight Ug-Value g-Value Light Transmission Sound Reduction
  nach EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 120
6
13.7
 
91
92
31
E(G) 30 - 120
8
18.2
 
90
92
32
E(G) 30 - 120
10
22.8
 
90
92
33
E(G) 30 - 120
12
27.4
 
90
92
34
*PYRAN® butt jointed glazing is available for fire rating E 30 and E 60

Contact

Mr. Martin Brown

SCHOTT UK Ltd.

Drummond Road
ST16 3EL Stafford
United Kingdom

 +44 (0)1785/223166
 +44 (0)1785/223522

At a glance

Areas of application

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

Product types

PYRAN® S

PYRAN® S is a monolithic, thermally tempered borosilicate safety glass in accordance with DIN EN Standard 13024-1. Thanks to its outstanding optical and mechanical properties, it has a long record of proven performance in many different buildings as a component in fire resistant glazing of the fire resistance classes E 30, E 60, E 90 and E 120.

  • Borosilicatglass
  • Classifications:
  • E 30 to E 120
  • EW 30 to E 60
  • Glass thickness: up to 12 mm

Design and variety of PYRAN® S

    PYRAN® S - Anti-reflective glazing

    PYRAN® S for anti-reflective glazing performs several important functions all at the same time. It offers clear visibility due to low residual reflection and up to 2 hours of additional protection in case of fire. Anti-reflective coated PYRAN® S is a monolithic, thermally toughened borosilicate glass that is anti-reflective on both sides due to the fact that it is manufactured using a dip-coating process. The glass is coated with a hard, weather-resistant and multi-layered interference system. As a result, light reflection of 8% with an uncoated glass can be reduced to 1% using coated borosilicate glass.

    PYRAN® S - Butt joint system

    Butt joint PYRAN® S can be used very easily in demanding architectural designs. With the PYRAN® S butt joint system, for instance, a special silicone joint is used to join the panes of glass together without a frame. This helps create light, smooth sheets of glass that are virtually endless, and guarantees a clear view at all times without any disturbing vertical profiles. Simply ideal for applications in which fire protection needs to be combined with maximum visibility and minimal visual disturbances.

    PYRAN® S - Structural glazing

    Systems that use PYRAN® S for structural glazing require no frame constructions whatsoever. This is the result of a perfect symbiosis between glass panes connected to each other by joints that are barely noticeable and point mounts and brackets that secure the glass panes to a strong, yet light, supporting structure. The panes remain permanently fixed in place, free of tension and without slippage under even the most extreme conditions, such as loads created by internal wind pressure or suction.

    PYRAN® S – Composite safety glass

    PYRAN® S composite safety glass as a laminate made of PYRAN® S and soda lime or single-pane safety glass can be used to meet special requirements for noise protection and protection against falls.
    The use according to TRLV and TRAV is stipulated in the general type approval Z-70.3-145. In addition to certification of protection against falling, there are general type approval test certificates according to TRAV with timber or steel frames.

PYRAN® S – Technical data

TECHNICAL INFORMATION
Product Fire Rating Thickness Weight Ug-Value g-Value Light Transmission Sound Reduction
  nach EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 120
6
13.7
 
91
92
31
E(G) 30 - 120
8
18.2
 
90
92
32
E(G) 30 - 120
10
22.8
 
90
92
33
E(G) 30 - 120
12
27.4
 
90
92
34
*PYRAN® butt jointed glazing is available for fire rating E 30 and E 60

Mr. Martin Brown

SCHOTT UK Ltd.

Drummond Road
ST16 3EL Stafford
United Kingdom

 +44 (0)1785/223166
 +44 (0)1785/223522