PYRANOVA® used in standard laminates refers to a compact multi-pane composite glass which meets the requirements of fire resistance class EI. In case of fire, it provides effective protection against passage of fire, hot gases and smoke, as well as heat radiation, for up to two hours. PYRANOVA® secure effectively combines fire protection with resistance to impact and manual attack in accordance with DIN EN 356 and resistance to bullet attack in accordance with DIN EN 1063.

Technical data

Glastype Article number EN 356 EN 1063 Fire resistance class Thick-
ness in mm
Weight in kg/m2

Fire protection & Manual attack resistance - Standard products
PYRANOVA® secure 30 P4A 5.4.2 P4A - EI 30 21 52
PYRANOVA® secure 30 P5A 5.10.2 P5A - EI 30 22 52
PYRANOVA® secure 30 P6B 1.1.6 P6B - EI 30 20 45
PYRANOVA® secure 30 P7B 1.2.6 P7B - EI 30 21 46
PYRANOVA® secure 30 P8B 1.3.1 P8B - EI 30 23 48

Fire protection & Manual attack resistance -
Special products (suitable for panic doors RC 2 + RC 3)
PYRANOVA® secure 30 P8B PRC2 1.9.7 P8B P2 - EI 30 27 52
PYRANOVA® secure 30 P8B P3 1.11.81) P8B P3 - EI 30 31 61
PYRANOVA® secure 30 P8B PRC3 1.8.22) P8B PRC3 - EI 30 35 65

Fire protection & Bullet resistance - Standard products
PYRANOVA® secure 30 BR2NS 2.1.1   BR2NS EI 30 19 42
PYRANOVA® secure 30 BR2NS 10.0.12   BR2NS EI 30 34 75
PYRANOVA® secure 30 BR4NS 1.1.9 P8B BR4NS EI 30 28 61
PYRANOVA® secure 30 BR4NS 10.0.10 P8B BR4NS EI 45 /
EW 60
56 124
PYRANOVA® secure 30 BR4NS 9.0.113) P8B BR4NS EI 45 /
EW 60
52 114
1) suitable for panic doors WK 3
2) suitable for panicsdoors RC 3
3) only for indoor applications [Edit Content]

Downloads

News, Trade Fairs & Events
14.
January
Trade fair BAU, Munich, Germany, 14.01 - 19.01.2019
27.
June
Trade fair Sicherheitsexpo, München, Germany, 27.06 - 28.06.2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.