Our unique manufacturing process
gives PYRAN<sup>®</sup> Platinum its outstanding surface quality
Our unique manufacturing process gives PYRAN® Platinum its outstanding surface quality

PYRAN® PlatinumSuperior quality and clarity

Summary

PYRAN® Platinum F – At a glance

PYRAN® Platinum F is a fire-protection rated and impact safety-rated glazing material made from a transparent glass-ceramic with a thickness of 3/16” (5 mm). It has a surface applied safety film and is intended for use in safety rated locations such as door lites, transoms or sidelites, and windows with fire-rating requirements up to 90 minutes (up to 180 minutes in doors).

General Characteristics

  • Thickness: 3/16" (5 mm)
  • Weight: 2.5 lbs/ft²
  • Clear; No amber tint
  • Surface: Float glass quality with surface applied safety film
  • Maximum sheet sizes: 43" x 77"
  • Impact rating: ANSI Z97.1 and CPSC 16CFR1201 (Cat. I and II)

Key facts

PYRAN® Platinum F

PYRAN® Platinum F is a fire-protection rated and impact safety-rated glazing material made from a transparent glass-ceramic with a thickness of 3/16” (5 mm). It has a surface applied safety film and is intended for use in safety rated locations such as door lites, transoms or sidelites, and windows with fire-rating requirements up to 90 minutes (up to 180 minutes in doors).

  • Fire-rated up to 90 minutes (up to 180 minutes in doors) with required hose stream test
  • Specially floated glass-ceramic with surface applied safety film
  • Transparent and wireless
  • Withstands thermal shock
  • Approved for use with any fire-rated frame
  • Conforms to positive pressure test standards
  • Environmentally-friendly glass-ceramic; produced without hazardous heavy metals arsenic and antimony
  • Can be used to construct insulated glazing units
  • Can be lightly sandblasted or delivered with surface-applied opacity film
  • Available locally throughout North America

Technical data

Rating Location Max. exposed area of glazing (in²) Max. width of exposed glazing (in) Max. height of exposed glazing (in) Min. depth of groove (in) Groove Width (in) Building Code Marking
Up to 90 min Doors Non-Temp Rise
2,736
(19 ft²)
36
76
5/8
7/16,
3/18
D-H-90
Up to 180 min Doors Temp Rise and Non-Temp Rise
100
(0.69 ft²)
12
36
1/2
7/16,
3/18
D-H-180
Up to 90 min Transom lites, sidelites, windows
3,422
(23.7 ft²)
76
76
5/8
7/16,
3/18
OH-90

Classified and labeled by Underwriters Laboratories, Inc. for the United States and Canada with File-No. R22036. All fire tests performed in accordance with UL 9, UL 10C, UBC 7-2 (1997), UBC 7-4 (1997), NFPA 257, NFPA 80, ASTM E2010-01, ASTM E2074-00, and ULC CAN4-S106.p>

Note: This product is not considered a barrier to radiant heat and has not met the ASTM E-119 or UL 263 test standards. All listing information is subject to change. The current listing can be accessed in the UL directory under file #R22036 or upon request from SCHOTT.


Labeling

After cutting, each lite of PYRAN® Platinum fire-rated glass-ceramic shall be permanently labeled according to local building code requirements with product and manufacturer’s name, UL certification mark, fire rating, etc.

Storage & Handling

PYRAN® Platinum fire-rated glass-ceramic should be handled with care during transportation, storage, inspection, and installation. It should be stored in dry conditions only and needs to be stacked upright or at a slight angle. In addition, the panels must be separated by an appropriate material, such as soft pads made of cork and the bottom edge must be supported along its entire length.

Installation

PYRAN® Platinum shall only be installed into fire-rated frame and window assemblies carrying the same rating. Each PYRAN® Platinum panel should be inspected carefully before installation, and any pieces with visible edge or surface damage should be sorted out. All glazing components and the stop height must be chosen according to the PYRAN® Platinum UL classification. The panel must be placed on calcium silicate or hardwood setting blocks and glazed using PYRAN® Platinum classified glazing tape, such as closed cell PVC, Fiberfrax tape or Pemko FG3000S90. The installation of the framed unit must comply with the frame supplier's instructions.

PYRAN® Platinum is a specially developed glass-ceramic, that fulfills the fire protection rating requirements. The production process may create certain optical imperfections, such as bubbles or knots. Since these do not generally impair the transparency or the technical performance of the glass-ceramic, they do not represent cause for rejection or replacement.

Maintenance & Care

To maintain the aesthetics, it is important to keep the panel clean. A soft, clean, non-abrasive cloth and a mild soap, detergent, or non-abrasive window cleaning solution is suitable for cleaning. After cleaning, rinse immediately with clean water and remove any excess water from the panel surface. Also, do not allow any metal or hard parts of the cleaning equipment to come in contact with the panel surface.

Contact

SCHOTT
Technical Glass Solutions GmbH

Otto-Schott-Strasse 13
07745 Jena
Germany

 +49 (0)3641/681-4666
 +49 (0)3641/28889-311

At a glance

PYRAN® Platinum F is a fire-protection rated and impact safety-rated glazing material made from a transparent glass-ceramic with a thickness of 3/16” (5 mm). It has a surface applied safety film and is intended for use in safety rated locations such as door lites, transoms or sidelites, and windows with fire-rating requirements up to 90 minutes (up to 180 minutes in doors).

General Characteristics

  • Thickness: 3/16" (5 mm)
  • Weight: 2.5 lbs/ft²
  • Clear; No amber tint
  • Surface: Float glass quality with surface applied safety film
  • Maximum sheet sizes: 43" x 77"
  • Impact rating: ANSI Z97.1 and CPSC 16CFR1201 (Cat. I and II)

Areas of application

Product types

PYRAN® Platinum F

PYRAN® Platinum F is a fire-protection rated and impact safety-rated glazing material made from a transparent glass-ceramic with a thickness of 3/16” (5 mm). It has a surface applied safety film and is intended for use in safety rated locations such as door lites, transoms or sidelites, and windows with fire-rating requirements up to 90 minutes (up to 180 minutes in doors).

  • Fire-rated up to 90 minutes (up to 180 minutes in doors) with required hose stream test
  • Specially floated glass-ceramic with surface applied safety film
  • Transparent and wireless
  • Withstands thermal shock
  • Approved for use with any fire-rated frame
  • Conforms to positive pressure test standards
  • Environmentally-friendly glass-ceramic; produced without hazardous heavy metals arsenic and antimony
  • Can be used to construct insulated glazing units
  • Can be lightly sandblasted or delivered with surface-applied opacity film
  • Available locally throughout North America

PYRAN® Platinum F – Technical data

TECHNICAL INFORMATION
Rating Location Max. exposed area of glazing (in²) Max. width of exposed glazing (in) Max. height of exposed glazing (in) Min. depth of groove (in) Groove Width (in) Building Code Marking
Up to 90 min Doors Non-Temp Rise
2,736
(19 ft²)
36
76
5/8
7/16,
3/18
D-H-90
Up to 180 min Doors Temp Rise and Non-Temp Rise
100
(0.69 ft²)
12
36
1/2
7/16,
3/18
D-H-180
Up to 90 min Transom lites, sidelites, windows
3,422
(23.7 ft²)
76
76
5/8
7/16,
3/18
OH-90

Classified and labeled by Underwriters Laboratories, Inc. for the United States and Canada with File-No. R22036. All fire tests performed in accordance with UL 9, UL 10C, UBC 7-2 (1997), UBC 7-4 (1997), NFPA 257, NFPA 80, ASTM E2010-01, ASTM E2074-00, and ULC CAN4-S106.p>

Note: This product is not considered a barrier to radiant heat and has not met the ASTM E-119 or UL 263 test standards. All listing information is subject to change. The current listing can be accessed in the UL directory under file #R22036 or upon request from SCHOTT.


Labeling

After cutting, each lite of PYRAN® Platinum fire-rated glass-ceramic shall be permanently labeled according to local building code requirements with product and manufacturer’s name, UL certification mark, fire rating, etc.

Storage & Handling

PYRAN® Platinum fire-rated glass-ceramic should be handled with care during transportation, storage, inspection, and installation. It should be stored in dry conditions only and needs to be stacked upright or at a slight angle. In addition, the panels must be separated by an appropriate material, such as soft pads made of cork and the bottom edge must be supported along its entire length.

Installation

PYRAN® Platinum shall only be installed into fire-rated frame and window assemblies carrying the same rating. Each PYRAN® Platinum panel should be inspected carefully before installation, and any pieces with visible edge or surface damage should be sorted out. All glazing components and the stop height must be chosen according to the PYRAN® Platinum UL classification. The panel must be placed on calcium silicate or hardwood setting blocks and glazed using PYRAN® Platinum classified glazing tape, such as closed cell PVC, Fiberfrax tape or Pemko FG3000S90. The installation of the framed unit must comply with the frame supplier's instructions.

PYRAN® Platinum is a specially developed glass-ceramic, that fulfills the fire protection rating requirements. The production process may create certain optical imperfections, such as bubbles or knots. Since these do not generally impair the transparency or the technical performance of the glass-ceramic, they do not represent cause for rejection or replacement.

Maintenance & Care

To maintain the aesthetics, it is important to keep the panel clean. A soft, clean, non-abrasive cloth and a mild soap, detergent, or non-abrasive window cleaning solution is suitable for cleaning. After cleaning, rinse immediately with clean water and remove any excess water from the panel surface. Also, do not allow any metal or hard parts of the cleaning equipment to come in contact with the panel surface.

SCHOTT
Technical Glass Solutions GmbH

Otto-Schott-Strasse 13
07745 Jena
Germany

 +49 (0)3641/681-4666
 +49 (0)3641/28889-311