PYRAN® G

At a glance

Whereas panes arranged in a facetted formation create an interrupted appearance, curved PYRAN® G components offer a clear, complete visual outlook. PYRAN® G is a monolithic, thermally tempered borosilicate glass. A forming process is used to give PYRAN® G its typical cylindrical shape. PYRAN® G offers outstanding transparency combined with visually stunning design when used in fire resistant glazing that meets the requirements of fire resistance class E 30.
  • Borosilicate glass
  • Classifications:E 30
  • Max. size:
    1200 mm x 2000 mm or 1000 mm x 2300 mm
  • Glass thickness:
    5, 6 and 8 mm

Technical data

Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
  acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® G E 30
5
11.4
  91
92
30
E 30
6
13.7
 
91
92
31
E 30
8
18.2
 
90
92
32