OPALIKA®OPALIKA® is a translucent white opal glass that distributes light evenly and naturally.
ARTISTA®ARTISTA® is a decorative color glass for aesthetic interior and exterior applications.
IMERA®IMERA® is a body-tinted glass with a smooth fire-polished surface. It is available in multiple color shades.
RIVULETTA®RIVULETTA® is a highly transparent, colorless, machine-drawn flat glass with a surface pattern of finely defined parallel lines on one side.
MIRONA®When the space behind the glass is dark, MIRONA® glass is an elegant mirror; however, when it from behind it is transformed into a transparent window.
NARIMA®NARIMA® glass produces dazzling color effects in six different variations creating a bold visual statement.
|