Colored glasses are becoming more and more popular as a design tool in architecture. Here, the surface generally determines the area of application. Whether for interior use, such as furniture and door glazing,
partitions or shower cabinets or outdoors in facades, colored glass creates the perfect atmosphere. In fact, the glazing itself offers potential for making decorating decisions. This makes it possible to set attractive
colorful accents, particularly in commercial buildings.
|
ARTISTA® for architectural applications
|
 |
Novartis Headquarter "Forum 3", Basel
|
ARTISTA® is a body-tinted Fourcault Glas with a textured surface on one side. The consistent exactly specified and intense color shades are characteristically for this glass. ARTISTA® can be processed in the same way as conventional glass. For this reason, ARTISTA® is not only suited for use in colored glass applications involving larger surface areas, but also in architecture, where it offers a variety of different ways to create designs and set attractive colorful accents - both indoors and outside.
|
ARTISTA® for fusing application
|
 |
SCHOTT Headquarter, Mainz
|
ARTISTA® opens the door to a variety of new possibilities. Special types of glasses in various formats and colors are placed onto a larger pane of glass and melted inside a kiln.
The results: exceptional brilliance of color and smooth transitions between the melted areas. ARTISTA® is currently the only fusible glass that is also suitable for creating larger formats.
It can also be processed into either laminated safety glass or insulation glass.
|
ARTISTA® - Frits & Thin glasses
|
ARTISTA® Frits and Thin Glasses open up a much wider spectrum of possibilities with respect to both design and safety. These products enable even fused glasses to be tempered into safety glass.
|
|