Stay cool, calm & collected
|
PYRANOVA® is a clear, laminated composite glass,
consisting of at least two float glass panes. A transparent fire resistant layer, which foams in
the case of fire, is incorporated between the panes. PYRANOVA®, applied in fire resistant glazing for integrity and insulation
verhindert PYRANOVA® avoids
the passage of fire, smoke and heat radiation.Fire resistant glazing by PYRANOVA® provides
the following distinctive properties:- Enduring transparency and stability,
ambient temperature from -20 °C to 50 °C
- Good sound insulation properties
- In accordance with EN 13501, PYRANOVA®
provides up to 60 minutes insulation and
integrity against flames, smoke and heat
radiation from the fire to the non-fire side of
the glazing
- PYRANOVA® has also been tested for impact
resistance in accordance with EN12600 and
has achieved a rating of Class 1 (B) 1
- PYRANOVA® can be provided in combination
with a range of glass types in addition to the
standard clear float sheets
|
PYRANOVA® fire resistant glass will act as a barrier against spread
of fire, smoke and heat radiation. The float glass pane facing the
fire shatters. The enclosed, transparent fire resistant layers foam up
and form an opaque heat shield, which prevents the passage of
heat radiation. Depending on the thickness of the composite, the
fire resistance time can be influenced accordingly.
|
PYRANOVA® is suitable for all areas of buildings
requiring protection from fire.
In co-operation
with system partners, SCHOTT JENAer GLAS
GmbH develops internationally approved constructions
with PYRANOVA®, which are ideally suited for
application in:- doors
- facades as well as
- butt jointed partition walls,
such as on escape routes and stairways.
|
| Fire Resistance Category |
Frame material / system |
| steel |
timber |
aluminium |
butt joint |
Planline |
| EI 30 |
x |
x |
x |
x |
x |
| EI 60 |
x |
x |
|
x |
|
|
|
Contact
SCHOTT AG
Hattenbergstrasse 10 55122 Mainz Germany
| +49 (0)6131/66-0 |
| +49 (0)6131/66-2000 |
E-mail
More contacts
|