MEMpax®

MEMpax® is available as:

Supply Forms
Thicknesses*
Standard Thicknesses*
Dimensions
  • Wafers
  • Substrates
0.1 mm to 0.5 mm 0.2 mm, 0.3 mm, 0.4 mm, 0.5 mm 2" to 12", round or rectangular
* Other thicknesses available upon request.