Supply Forms and Geometrical Tolerances
Nominal thickness1) in μm 50, 70, 100, 145, 175, 210, 250, 330, 350, 400
Format2) in mm x mm 500 x 400
440 x 360
Cut-to-size format2) in mm x mm rectangular: 5~580
round: Ø 50~410
Thickness tolerance3) in μm ± 10
TTV3) in μm ≤ 10
Warp3) in μm  ≤ 100 - ≤ 1000 ≤ 100 - ≤ 1000
Roughness in nm  < 0.5