Fused Silica Lithosil®


Product Information



High quality synthetic fused silica LITHOSIL® with excellent optical properties is particularly suitable for the highly demanding applications found in the optical industry. The different quality levels (offered in different grades: Q0, Q1, Q2, QT) can be adapted to all kinds of individual customers' needs, from NIR (IR) to DUV.

Synthetic fused silica from SCHOTT LITHOTEC has the following outstanding properties:
  • Free of inclusions and bubbles (eg. grades Q0 + Q1)
  • Excellent UV transmittance from 185 nm to 2.5 µm
  • High laser durability
  • High refractive index homogeneity: additional 3D option
  • High temperature stability
  • Low stress birefringence
  • Very low thermal expansion coefficient
  • Very low fluorescence


Benefits

The amorphous synthetic fused silica LITHOSIL® of high purity completes the application range of optical materials from DUV to IR with a very good transmission ranging from 185 nm to 2.5 µm.

Key Applications

Fused silica is widely used in applications such as:
  • Micro-/Lithographic applications: stepper lenses, photo mask blanks
  • DUV laser components
  • Standard optics
  • Excimer laser optics
  • Litho optics
  • Beam deliveries
  • Light pipes
  • Laser fusion
  • Technical usage


Forms of Supply

SCHOTT LITHOTEC offers LITHOSIL® components and blanks in different grades along with different surface qualities (raw, cut, ground or polished), depending on the individual requirements of the customers.

Specifications

Grades:
Different material grades are characterized in the functional direction by:
  • Very low inclusion / bubble levels
  • Low levels of refractive index variations and local in-homogeneities especially striae
Excimer Grades:
Excimer laser optics require fused silica of the following exceptional qualities:
  • High internal transmission, wide spectral UV-range
  • Very low fluorescence (qualified by laser induced fluorescence at 193 nm).
    Excimer grades are available in LITHOSIL® Q0 and Q1 grade
3D Material
  • Refractive index homogeneity qualified in all 3 dimensions depending on geometry
  • Available in LITHOSIL® Q0 grade
  • 3D Material is available on request


Quality Assurance

SCHOTT LITHOTEC offers fused silica with 100% control of homogeneity, stress birefringence, striae, bubbles, and inclusions. We utilize statistical control of refractive index, transmittance, laser induced fluorescence, trace-elements and OH-content.

Quality levels:
  • Q0: is characterized by its high three-dimensional optical homogeneity. Free of striations in any functional direction, it is recommended for high-end resolution requirements in optical elements such as prisms and lenses.
  • Q1: exhibits high homogeneity and has no striations in the functional direction. Typical applications are optical elements such as lenses, windows and wafers.
  • Q2: is not specified concerning homogeneity. This grade is recommended for optics in the visible spectral range or optics in the UV with less stringent demands on transmission.
  • QT: is not specified concerning homogeneity, striae and striations. This grade is recommended for technical applications.