Product Information

Low transformation temperatures suitable for precision molding

Precision molding is one of the state-of-the-art-technologies for the volume production of complex lenses (e. g. aspheres), for various applications.

SCHOTT offers several optical glasses specifically developed for precision molding – the low Tg glasses, such as P-SF68, P-SK57Q1, P-SK58A and P-BK7.

Low Tg glasses have a glass transformation temperature suitable for precision molding and a special glass composition to decrease the tendency for devitrification and to reduce the reaction with mold materials within the molding temperature range.

During precision glass molding, a polished or fire polished preform is shaped into a final geometry, while conserving its surface quality. The typical temperature range for the molding process is between 500 °C and 700 °C, enabling the extension of the operating lifetime of the mold material and a significant time reduction of the press process.

SCHOTT low Tg glasses are provided in the form of optical glass rods as well as ball lenses in different formats.

Advantages

  • Low transformation temperatures, mostly below 550 °C, to increase lifetime of molds and to reduce process time
  • Low tendency for chemical interaction between glass constituents and mold materials within the molding temperature range
  • Tight optical tolerance
  • Wide range of dimensions
  • Various forms of supply
  • Application support

Supply Forms

Low Tg glass for precision molding is available as:
 
Supply Forms*
Dimensions*
Optical glass rods
  • various shapes
  • various surface qualities
Diameter: < 1 mm - 7.5 mm; length: up to 1,000 mm
Diameter: > 7.5 mm - 12.5 mm; length: up to 140 mm
Ball lenses
  • different formats

Diameter: 0.8 mm - 14 mm

* Other supply forms and dimensions upon request. Please contact us.

Technical Information

Materials used

Low Tg Glasses in our Abbe-Diagram
业务联系
肖特(上海)精密材料和设备国际贸易有限公司
上海市虹梅路1801号凯科国际大厦301室
邮编:200233
中国
邮件联系+86 (0)21 3367 8000
新闻,展会与活动
14.
March
展会 LOPEC, Munich, Deutschland, 14.03 - 15.03.2018
06.
March
展会 IT Trans, Karlsruhe, Deutschland, 06.03 - 08.03.2018
改动
SCHOTT在本网站上使用Cookies来提高用户体验,并提供可能的最佳服务。一旦浏览本网站,即表示您同意我们使用Cookies。